A quantum chemical study of ZrO2 atomic layer deposition growth reactions on the SiO2 surface

Joseph H. Han, Guilian Gao, Yuniarto Widjaja, Eric Garfunkel, Charles B. Musgrave

Research output: Contribution to journalArticle

40 Citations (Scopus)

Abstract

Zirconium oxide (ZrO2) is one of the leading candidates to replace silicon oxide (SiO2) as the gate dielectric for future generation metal-oxide-semiconductor (MOS) based nanoelectronic devices. Experimental studies have shown that a 1-3 monolayer SiO2 film between the high permittivity metal oxide and the substrate silicon is needed to minimize electrical degradation. This study uses density functional theory (DFT) to investigate the initial growth reactions of ZrO2 on hydroxylated SiO2 by atomic layer deposition (ALD). The reactants investigated in this study are zirconium tetrachloride (ZrCl4) and water (H2O). Exchange reaction mechanisms for the two reaction half-cycles were investigated. For the first half-reaction, reaction of gaseous ZrCl4 with the hydroxylated SiO2 surface was studied. Upon adsorption, ZrCl4 forms a stable intermediate complex with the surface SiO2-OH* site, followed by formation of SiO 2-O-Zr-Cl* surface sites and HCl. For the second half-reaction, reaction of H2O on SiO2-O-Zr-Cl* surface sites was investigated. The reaction pathway is analogous to that of the first half-reaction; water first forms a stable intermediate complex followed by evolution of HCl through combination of a Cl atom from the surface site and an H atom from H2O. The results reveal that the stable intermediate complexes formed in both half-reactions can lead to a slow film growth rate unless process parameters are adjusted to lower the stability of the complex. The energetics of the two half-reactions are similar to those of ZrO 2 ALD on ZrO2 and as well as the energetics of ZrO 2 ALD on hydroxylated silicon. The energetics of the growth reactions with two surface hydroxyl sites are also described.

Original languageEnglish
Pages (from-to)199-212
Number of pages14
JournalSurface Science
Volume550
Issue number1-3
DOIs
Publication statusPublished - Feb 10 2004

Fingerprint

Atomic layer deposition
atomic layer epitaxy
Silicon
Metals
Atoms
Nanoelectronics
Water
Gate dielectrics
Silicon oxides
Film growth
Zirconium
Zirconia
Hydroxyl Radical
Oxides
Density functional theory
Monolayers
Permittivity
Adsorption
Degradation
tetrachlorides

Keywords

  • Density functional calculations
  • Growth
  • Halides
  • Silicon
  • Silicon oxides
  • Surface chemical reaction
  • Zirconium

ASJC Scopus subject areas

  • Physical and Theoretical Chemistry
  • Condensed Matter Physics
  • Surfaces and Interfaces

Cite this

A quantum chemical study of ZrO2 atomic layer deposition growth reactions on the SiO2 surface. / Han, Joseph H.; Gao, Guilian; Widjaja, Yuniarto; Garfunkel, Eric; Musgrave, Charles B.

In: Surface Science, Vol. 550, No. 1-3, 10.02.2004, p. 199-212.

Research output: Contribution to journalArticle

Han, Joseph H. ; Gao, Guilian ; Widjaja, Yuniarto ; Garfunkel, Eric ; Musgrave, Charles B. / A quantum chemical study of ZrO2 atomic layer deposition growth reactions on the SiO2 surface. In: Surface Science. 2004 ; Vol. 550, No. 1-3. pp. 199-212.
@article{f185fe7da2a443a3af1464b7cce27fb6,
title = "A quantum chemical study of ZrO2 atomic layer deposition growth reactions on the SiO2 surface",
abstract = "Zirconium oxide (ZrO2) is one of the leading candidates to replace silicon oxide (SiO2) as the gate dielectric for future generation metal-oxide-semiconductor (MOS) based nanoelectronic devices. Experimental studies have shown that a 1-3 monolayer SiO2 film between the high permittivity metal oxide and the substrate silicon is needed to minimize electrical degradation. This study uses density functional theory (DFT) to investigate the initial growth reactions of ZrO2 on hydroxylated SiO2 by atomic layer deposition (ALD). The reactants investigated in this study are zirconium tetrachloride (ZrCl4) and water (H2O). Exchange reaction mechanisms for the two reaction half-cycles were investigated. For the first half-reaction, reaction of gaseous ZrCl4 with the hydroxylated SiO2 surface was studied. Upon adsorption, ZrCl4 forms a stable intermediate complex with the surface SiO2-OH* site, followed by formation of SiO 2-O-Zr-Cl* surface sites and HCl. For the second half-reaction, reaction of H2O on SiO2-O-Zr-Cl* surface sites was investigated. The reaction pathway is analogous to that of the first half-reaction; water first forms a stable intermediate complex followed by evolution of HCl through combination of a Cl atom from the surface site and an H atom from H2O. The results reveal that the stable intermediate complexes formed in both half-reactions can lead to a slow film growth rate unless process parameters are adjusted to lower the stability of the complex. The energetics of the two half-reactions are similar to those of ZrO 2 ALD on ZrO2 and as well as the energetics of ZrO 2 ALD on hydroxylated silicon. The energetics of the growth reactions with two surface hydroxyl sites are also described.",
keywords = "Density functional calculations, Growth, Halides, Silicon, Silicon oxides, Surface chemical reaction, Zirconium",
author = "Han, {Joseph H.} and Guilian Gao and Yuniarto Widjaja and Eric Garfunkel and Musgrave, {Charles B.}",
year = "2004",
month = "2",
day = "10",
doi = "10.1016/j.susc.2003.12.030",
language = "English",
volume = "550",
pages = "199--212",
journal = "Surface Science",
issn = "0039-6028",
publisher = "Elsevier",
number = "1-3",

}

TY - JOUR

T1 - A quantum chemical study of ZrO2 atomic layer deposition growth reactions on the SiO2 surface

AU - Han, Joseph H.

AU - Gao, Guilian

AU - Widjaja, Yuniarto

AU - Garfunkel, Eric

AU - Musgrave, Charles B.

PY - 2004/2/10

Y1 - 2004/2/10

N2 - Zirconium oxide (ZrO2) is one of the leading candidates to replace silicon oxide (SiO2) as the gate dielectric for future generation metal-oxide-semiconductor (MOS) based nanoelectronic devices. Experimental studies have shown that a 1-3 monolayer SiO2 film between the high permittivity metal oxide and the substrate silicon is needed to minimize electrical degradation. This study uses density functional theory (DFT) to investigate the initial growth reactions of ZrO2 on hydroxylated SiO2 by atomic layer deposition (ALD). The reactants investigated in this study are zirconium tetrachloride (ZrCl4) and water (H2O). Exchange reaction mechanisms for the two reaction half-cycles were investigated. For the first half-reaction, reaction of gaseous ZrCl4 with the hydroxylated SiO2 surface was studied. Upon adsorption, ZrCl4 forms a stable intermediate complex with the surface SiO2-OH* site, followed by formation of SiO 2-O-Zr-Cl* surface sites and HCl. For the second half-reaction, reaction of H2O on SiO2-O-Zr-Cl* surface sites was investigated. The reaction pathway is analogous to that of the first half-reaction; water first forms a stable intermediate complex followed by evolution of HCl through combination of a Cl atom from the surface site and an H atom from H2O. The results reveal that the stable intermediate complexes formed in both half-reactions can lead to a slow film growth rate unless process parameters are adjusted to lower the stability of the complex. The energetics of the two half-reactions are similar to those of ZrO 2 ALD on ZrO2 and as well as the energetics of ZrO 2 ALD on hydroxylated silicon. The energetics of the growth reactions with two surface hydroxyl sites are also described.

AB - Zirconium oxide (ZrO2) is one of the leading candidates to replace silicon oxide (SiO2) as the gate dielectric for future generation metal-oxide-semiconductor (MOS) based nanoelectronic devices. Experimental studies have shown that a 1-3 monolayer SiO2 film between the high permittivity metal oxide and the substrate silicon is needed to minimize electrical degradation. This study uses density functional theory (DFT) to investigate the initial growth reactions of ZrO2 on hydroxylated SiO2 by atomic layer deposition (ALD). The reactants investigated in this study are zirconium tetrachloride (ZrCl4) and water (H2O). Exchange reaction mechanisms for the two reaction half-cycles were investigated. For the first half-reaction, reaction of gaseous ZrCl4 with the hydroxylated SiO2 surface was studied. Upon adsorption, ZrCl4 forms a stable intermediate complex with the surface SiO2-OH* site, followed by formation of SiO 2-O-Zr-Cl* surface sites and HCl. For the second half-reaction, reaction of H2O on SiO2-O-Zr-Cl* surface sites was investigated. The reaction pathway is analogous to that of the first half-reaction; water first forms a stable intermediate complex followed by evolution of HCl through combination of a Cl atom from the surface site and an H atom from H2O. The results reveal that the stable intermediate complexes formed in both half-reactions can lead to a slow film growth rate unless process parameters are adjusted to lower the stability of the complex. The energetics of the two half-reactions are similar to those of ZrO 2 ALD on ZrO2 and as well as the energetics of ZrO 2 ALD on hydroxylated silicon. The energetics of the growth reactions with two surface hydroxyl sites are also described.

KW - Density functional calculations

KW - Growth

KW - Halides

KW - Silicon

KW - Silicon oxides

KW - Surface chemical reaction

KW - Zirconium

UR - http://www.scopus.com/inward/record.url?scp=0942300334&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0942300334&partnerID=8YFLogxK

U2 - 10.1016/j.susc.2003.12.030

DO - 10.1016/j.susc.2003.12.030

M3 - Article

VL - 550

SP - 199

EP - 212

JO - Surface Science

JF - Surface Science

SN - 0039-6028

IS - 1-3

ER -